Practice of Process for VOD Nitrogen Bottom-Blown Refining High Nitrogen Steel P91
Guo Chang, Lil Wenjun, Zhou Lixin, Zhang Zhicheng, Yu Yaping , Ke Lin
Special Steel . 2011, (3): 48 -50 .