Transformation Behavior of Hot Continuous Rolling E36 Ship Plate during Continuous Cooling
Hu Hai , Zhao Gang , Bao Siqian , Ye Chuanlong , Xiong Xiangjiang, Li Lingling, Yang Xiaojun
Special Steel . 2011, (3): 58 -60 .