ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Effect of Rolling Process on Structure, Texture and Properties of X80 Pipeline Steel
Han Le , Sun Hao , Ren Huiping , Wang Haiyan , Jin Zili