Evolution of Structure and Texture in 3 % Si Steel during Hot and Cold Rolling Process based on CSP Technology
Yan Zhifei , Jin Zili , Ji Yunping , Liu Pengcheng , Zhang Libo
Special Steel . 2012, (2): 65 -67 .