Process Practice to Prevent Edge Crack of 5 mm Hot Continuous-Rolled Strip Coil of S31803 Duplex Stainless Steel
Li Guoping, Zhang Wei, Li Jun, Fan Xinzhi
Special Steel . 2010, (1): 36 -37 .