Effect of Non-Vacuum Nitrogen Blowing Process on Nitrogen Absorption Behavior of Austenite Stainless Steel 316L
Shi Yanlin , Bao Yanping , Dong Zhongqi
Special Steel . 2011, (5): 5 -7 .