ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

A Study on Simulation of Fluid Flowing and Inclusions Removing for Liquid Steel in Tundish with Bottom Gas Blowing
Li Xiaobing, Chen Weiqing , Cui Huaizhou , Wang Guangshun, Gao Yongbin