Experimental Research on Fine Reduction of EAF Dust at Xinyesteel
Wang Yujiao , Fan Xinyou , Li Shiqi , Sun Lingzhi , Gao Jintao , Jin Xiaohui , Liu Runzao , Qian Gang , Chen Changxi
Special Steel . 2011, (5): 18 -21 .