Practice for Control of Longitudinal Surface Crack of Q235B and Q345B Steel Casting Slab Produced by CSP Process
Cheng Zewei , Wang Yongsheng, Ruan Qiang, Cheng Dongquan
Special Steel . 2010, (3): 24 -26 .