Elevated Temperature Performance of Casting Slab of High Strength Weather-Resisting Steel Q450NQR1
Li Jianquan , Yang Subo , Gao Xingjian, Chen Dengfu, Song Liwei, Bi Yanyan
Special Steel . 2010, (3): 54 -56 .