An Analysis on Desulphurizing Efficiency during 110 t EBT EAF-LF-RH-CC Process for Production of Seamless Tube Steel 12MnV
Wang Jinghui, Li Jingshi, Jiang Guilian, Sun Haibo, Zheng Quanzhen
Special Steel . 2011, (2): 30 -33 .