ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Effect of Patenting Process on Structure and Properties of 70 Steel Wire
Dong Shufeng , Zhao Gang , Ye Chuanlong , Bao Siqian, Liu Jianbing, Li Junhong, Liu Xiaoping
Special Steel . 2011, (2): 60 -62 .