Practice of Continuous Rolling Process to Improve Macrostructure of Small Size Bar Products of Bearing Steel GCrl5
Fu Junwei , Zhao Jie , Liu Jianpei , Zhou Jianying
Special Steel . 2010, (5): 42 -44 .