Effect of Fluxing Agent B 2O 3 on Melting Temperature of CaO-Based Refining Slag
Wang Hongming , Ni Dongsheng , Zhao Hu , Li Guirong, Li Bo
Special Steel . 2009, (6): 1 -3 .