ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Behavior and Control of Nitrogen in Structural Steels Steelmaking by 100 t BOF-LF-RH-CC Process
Lu Jinxiang, Wang Zhongying, Chen Shuisheng , Xue Zhengliang, Ke Chao
Special Steel . 2009, (6): 26 -28 .