Heat Treatment Process and Structure of a Low Carbon Super-high Strength Quenching and Partitioning Steel Plate
Dong Chen , Jiang Haitao , Chen Yulai , Tang Di , Cheng Zhisong
Special Steel . 2009, (5): 68 -70 .