Influence of Cerium on Hot Workability of Super Duplex Stainless Steel 00Cr25Ni7Mo4N
Yu Fei, Song Zhigang, Zheng Wenjie, Guo Zhongcheng , Ji Xiangmin, Feng Han⊃2;
Special Steel . 2010, (4): 58 -60 .