Influence of Hot Deformation Process on Network Carbide of 100Cr6 Bearing Steel Wire
Zuo Jinzhong, He Xi, Zhao Yang, Zhou Yuan, Chen Tingjun
Special Steel . 2022, (6): 60 -65 .  DOI: 10.20057/j.1003-8620.2022-00167