Calculating Model for Nitriding and Denitriding of Stainless Steel 304 in AOD Refining and Its Application
Shen Chunfei , Jiang Xingyuan , Yin Shiyou , Jiang Zhouhua , Li Yang
Special Steel . 2009, (5): 28 -30 .