ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Analysis on Action and Reaction Force between Slab and Rollers at Segment of Dynamic Soft Reduction and Application in Casting
Xie Changchuan, Wang Xinhua , Zhang Jiongming , Li Fushuai , Wang Chaoying , Ai Jian , Jiao Yushui , Chen Maojin
Special Steel . 2009, (5): 22 -24 .