A Study of Water Model for Effect of Ladle Bottom Argon Blowing Position on Inclusion Removal from Liquid Steel
Chen Xiangyang, Zheng Shuguo , Dong Jie, Zhu Miaoyong
Special Steel . 2009, (3): 7 -9 .