Effect of Solution C on Bake Hardening Behavior of Nb-Ti Microalloying ULC-BH Steel Plate
Cui Yan, Wang Ruizhen, Yong Qilong, Li Haizhao
Special Steel . 2009, (3): 13 -15 .