ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

A Study on Aging Dynamics of Maraging Stainless Steel 00Cr13Ni7Mo4Co4W2Ti
Jiangue, Zhen Caixia, Li Caixia
Special Steel . 2009, (1): 4 -6 .