ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Effect of Cycle Plasma Nitriding Process on Structure and Properties of Nitrided Layer of Steel 38CrMoAl
Chen Wei, Wang Lei, Fu Yongtao, Yan Xiang
Special Steel . 2009, (6): 55 -57 .