Effect of Hot Deformation on Structure and Microhardness of 0.05C-0.13Nb Steel
Yin Shubiao, Liu Qingyou, Zhang Zhibo, Sun Xinjun, Lei Ting
Special Steel . 2008, (1): 25 -27 .