Study on the Absorption of TiN by the Mold Slag of High Titanium Welding Wire Steel
Wang Shisong, Zhang Xubin, Wang Yunbo, Jin Hebin, Wang Wei, Tang Qing
Special Steel . 2023, (3): 46 -52 .  DOI: 10.20057/j.1003-8620.2022-00151