ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Advance in Production Technology of Cold Rolled Grain-Oriented Electrical Steels
Xia Zhaosuo, Kang Yonglin, Wang Quanli
Special Steel . 2007, (6): 35 -38 .