Calculation of Specific Interfacial Energy and Ripening Rate for Cooper in Ferrite of Bainite Steel
Li Guangmin , Yan Huicheng , Qiu Shengtao , Yong Qilong , Xiang Jinzhong
Special Steel . 2008, (5): 16 -18 .