ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Practice of Pilot Production on Φ600 mm Continuous Casting Round Bloom of 4130X Steel for Large Volume Seamless Gas Cylinders
Li Gang, Ding Wenbin, Zhang Chaolei, Yin Xiugang, Yao Zhong
Special Steel . 2022, (1): 44 -46 .