Affecting Factors Analysis and Numerical Simulation for Hot Charging of Cast Bloom of Heavy Rail Steel
Li Feng , Shi Fengwu , Dong Zhen , Liu Ping , Chen Aimei , Lan Yueguang
Special Steel . 2008, (5): 52 -53 .