Effect of Cold Treatment Temperature on Structure and Mechanical Properties of Steel 1Cr20Co6Ni2WMoV
Zhang Hong, Wang Limin, Yang Gang, Liu Rongpei, Liu Ning
Special Steel . 2007, (1): 35 -37 .