Effect of Open-Die Forging Process and Carbon Content on Microstructure and Mechanical Properties of High-temperature Alloy GH3128
Li Chenglong, Zhong Yuguo, Li Qing, Zhao Changhong, Rong Wenkai
Special Steel . 2023, (3): 90 -93 .  DOI: 10.20057/j.1003-8620.2022-00192