Nb and Heat Treatment on Structure and Properties of C-Mn-Si Series Cold Rolled Dual Phase Steel
Zhang Zengliang, SongRenbo, Cheng Zhisong, Zhao Zhenghi, Zha Aimin, Liu Guangning, Xiong Aiming
Special Steel . 2008, (2): 13 -15 .