Effect of Boron on Hot Workability,Structure and Mechanical Properties of Austenite Heat Resistant Steel TP347H
Xu Gang', Li Jun', Xiao Xueshan, Ni Jiansen, Zhu Changchun, Zhao Junliang, Zheng Wei and Wang Zhizheng
Special Steel . 2008, (2): 23 -25 .