Control of Oxygen Content in 20MnCr5 Gear Steel and Its Effect on Fatigue Performance of Steel
Cao Hongfu , Wang Maoqiu , Sun Hongping , He Xiaofei , Wu Shaoguang
Special Steel . 2023, (1): 1 -4 .  DOI: 10.20057/j.1003-8620.2022-00045