Effect of Electroslag Remelting in Protective Atmosphere on Composition and Inclusions of DZ2 High⁃Speed Axle Steel
Wu Zhonghua , Guo Bo , Wang Songwei , Wang Yutian , Zhang Jinwen
Special Steel . 2023, (1): 15 -24 .  DOI: 10.20057/j.1003-8620.2022-00033