An Analysis on Failure of Centrifugal Casting Radiant Tubes of Austenite Heat Resistant Steel HP40
Zhang Xiaoli, Luo Heli, Li Shangping, Liu Peiying and Zhou Tietao
Special Steel . 2008, (2): 65 -66 .