Application of Particle Injection Dephosphorization Process on Steelmaking of 130 t Electric Arc Furnace
Chen Junzhao, Zhang Yanhui , Tan Antong , Li Likai, Kang Jianguang
Special Steel . 2023, (1): 34 -38 .  DOI: 10.20057/j. 1003-8620.2022-00073