Pitting Erosion Analysis of Ultra-Pure Ferritic Stainless Steel 445J2 and 316L Ultra-Low-Carbon Austenitic Stainless Steel in Lithium Bromide Solution
Wu Zhuojie, Hou Lifeng, Du Huayun, Zou Yong, WuMin, Fan Guangwei, Wei Yinghui,
Special Steel . 2023, (1): 65 -71 .  DOI: 10.20057/j.1003-8620.2022-00069