Microstructure and Properties of Low-nickel Austenitic Stainless Steel14.0Cr-1.1Ni-9.2Mn-0.30Cu
Wu Hailin, Chen Xiaolong, Qian Xuehai, Zeng Yao, Chen Shenglin
Special Steel . 2023, (1): 72 -77 .  DOI: 10.20057/j.1003-8620.2022-00055