Effect of Solution Temperature and Grain Size on Ultra Low Temperature Impact Energy of S31608 Stainless Steel Extruded Pipe
Wang Shaobing, Sun Wenqiang, Wang Man, Zhou Zhu, Du Lei, Lu Qianqian
Special Steel . 2023, (1): 89 -92 .  DOI: 10.20057/j.1003-8620.2022-00038