ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Physical Simulation on Bubbles Movement in Mold for Slab with Nozzle Argon Injection Process
Feng Wei , Hu Mingqian , Li Deqiang , Liu Chengjun , Jiang Maofa
Special Steel . 2007, (5): 28 -30 .