ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Math Model for Optimum Charge Partition on Stainless Steel Smelting by K-OBM-S Process
Xu Fanghong , Gong Wei , Jiang Zhouhua
Special Steel . 2007, (5): 51 -53 .