Mathematical Modeling of K-OBM-S Converter Melting Process for Steelmaking of Stainless Steel
Dong Yanwu , Jiang Zhouhua , Gong Wei , Li Jianmin , Chang Tianyin , Wang Yanming , Liu Weidong
Special Steel . 2006, (2): 13 -16 .