Effect of Different Alloying Processes on Inclusions of 18Cr Ultra-pure Ferrite Stainless Steel during Refining Process
Zhang Jianlong, Chen Xingrun, Cheng Yunxia, Li Hongliang, Xu Bin, Pan Jixiang
Special Steel . 2023, (3): 34 -38 .  DOI: 10.20057/j.1003-8620.2022-00207