Research and Production of Nb-Ti Microalloy Steel QStE380TM Hot Rolled Plate for Auto Beam by CSP Line
Wang Baofeng , Ding Guo , Zhao Liping , Wang Xuelian , Li Degang
Special Steel . 2006, (2): 49 -51 .