Analysis on Clogging of Submerged Entry Nozzle for 409L Stainless Steel Concasting and Improved Measure
Zheng Hongguang, Lu Bin, Li Shi, Wang Lijiang , Chen Xu
Special Steel . 2006, (6): 50 -51 .