Effect of Subcritical Treatment on Structure and Properties of High Strength Steel 40SiMnCrNiMo for Rock Drill Tools
Xu Xiang, Ji Kejin, Wang Bin, Cao Lin, Fang Jun
Special Steel . 2006, (6): 57 -58 .