A Short-cut Calculation Method for Finishing Rolling Temperature Control of Hot Rolled Strip
Gong Dianyao, Xu Jianzhong, Zheng Hui, Liu Xianghua, Wang Guodong
Special Steel . 2007, (2): 31 -33 .