Study and Application of Fuzzy Neural Network Model of Improved Training Method to Predict End Point Phosphorus
Liu Dongmei, Chen Bin, Wang Shuge, Zou Zongshu, Yu Aibing
Special Steel . 2007, (2): 41 -43 .